The instability of aqueous Zn metal anodes originates from the coupled failure of interfacial chemistry and deposition crystallography, where water-rich Helmholtz planes trigger parasitic reactions while disordered Zn nucleation accelerates dendrite growth. Conventional electrolyte additives mainly regulate solvation or interfacial adsorption, but rarely integrate Helmholtz plane reconstruction with crystallographic texture control. Herein, we propose a bioinspired zincophilic electrolyte engineering strategy using L-theanine (TN), a naturally derived biomolecule, to construct a dynamically stabilized anode-electrolyte interface. Spectroscopic analyses, in-situ diagnostics, molecular dynamics simulations, and density functional theory calculations demonstrate that TN coordinates with Zn 2+ , disrupts the Zn 2+ -H 2 O interaction, and reconstructs the outer Helmholtz plane by partially replacing coordinated water. Simultaneously, TN preferentially adsorbs at the inner Helmholtz plane and forms a water/sulfate-repellent interfacial layer, which suppresses hydrogen evolution, electrode corrosion, and zinc hydroxysulfate formation. Beyond chemical passivation, the TN-derived adaptive layer homogenizes interfacial ion flux and promotes Zn adatom self-diffusion, inducing dendrite-free Zn deposition with a favorable (002)-oriented texture. Consequently, Zn|TN-0.2|Zn cells operate stably for over 4000 h, and Zn|TN-0.2|Cu cells achieve an average Coulombic efficiency of 99.5% for 1400 cycles. Moreover, Zn|TN-0.2|I 2 @C full cells retain 95.2% capacity after 20,000 cycles at 10 A g −1 . This work advances electrolyte additive design from single-factor interfacial protection toward bioinspired molecular programming of both Helmholtz chemistry and Zn deposition texture.
No takes yet. Share an insight, caveat, or question.
Gou et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: