Demonstrates multi-octave frequency comb generation from ultraviolet to near-infrared in diamond crystals at cryogenic temperatures, indicating potential for ultrashort pulse synthesis.
We study stimulated Raman scattering (SRS) and Raman four-wave mixing (RFWM) processes in chemical vapour deposition (CVD) diamond crystals. The strong interaction of picosecond laser pulses at 1.064 and 0.532 µm wavelength with the dominant Raman-active F2g mode results in a more than two-octave-spanning frequency comb, ranging from the UV to the NIR spectral region. In addition to spectroscopic analysis of the χ(3)-nonlinear emission at room temperature, comparative measurements have been carried out at cryogenic temperature of 10 K. The Raman shift and the Raman gain are found to change only weakly. Moreover, the potential of SRS frequency comb generation in CVD diamond for ultra-short pulse synthesis is discussed.
No takes yet. Share an insight, caveat, or question.
Lux et al. (2014) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: