The objective of this paper is to examine the effects of Si and P in low carbon steels on surface hot shortness due to Cu. Susceptibility of the steels to surface hot shortness was evaluated by a new method using tensile tests which is proposed by the present authors. Tensile tests were carried out after heating specimens at 1 000, 1 100 and 1 200°C in air and in Ar gas. Tensile tests using specimens implanting a Cu rod, observation of oxidation rate by thermogravimetry, optical microscopy and EPMA of steel/scale interface region etc. were also performed. At 1 100°C, single additions of 0.4 % Si and 0.02 % P were effective to decrease susceptibility to surface hot shortness, although these increased the oxidation rate. Duplex addition of 0.4 % Si and 0.02 % P decreased the oxidation rate and exhibited a substantial effect on a decrease in the susceptibility. Addition of Si decreased the amount of Cu-enriched phase at steel/scale interface. This is contributable to the reduction of the susceptibility to surface hot shortness. Internal oxidation of Si is thought to decrease the amount of the Cu-enriched phase. Single addition of 0.02 % P seems to increase slightly the amount of the Cu-enriched phase. A critical stress exists to fracture the specimens by Cu-enriched liquid phase. The additions of Si and P increase this critical stress. Silicon also contributes to a decrease in the growth rate of the crack created by the penetration. At 1 200°C, the susceptibility to surface hot shortness in all steels decreased compared with that at 1 100°C, but trends of effects of single and duplex additions of 0.4 % Si and 0.02 % P on the susceptibility were similar to those at 1 100°C. The oxidation rate for all steels was much higher than at 1 100°C, but the amount of Cu-enriched phase at steel/scale interface was reduced compared with at 1 100°C. The amount of the Cu-enriched phase in the steels containing 0.4 % Si is smaller than that in other steels. Liquid phase which appears in scale at temperatures higher than 1 177°C (eutectic temperature of FeO-2FeO·SiO2) is a contributing factor in both increases of the oxidation rate and occlusion of Cu into the scale at 1 200°C.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Seo et al. (1997) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: