Doping concentration optimized CaSc2O4:0.004Tm3+/0.1Yb3+ shows stronger upconversion luminescence (UCL) than doping concentration also optimized typical oxide upconverting phosphor Y2O3:0.004Tm3+/0.1Yb3+ upon 980 nm laser diode pump. The two-step up converted 3H4 → 3H6 near infrared emission peaked around 800 nm and the three-step up converted 1G4 → 3H6 blue emission around 480 nm of Tm3+ is enhanced by a factor of 3.5 and 2.2, respectively. On analyzing the 2F5/2 → 2F7/2 emission intensities and decay curves of Yb3+ in the two hosts, we reveal that Yb3+ in CaSc2O4 exhibits both a larger absorption cross section at 980 nm and Yb3+ → Tm3+ first step energy transfer coefficient (9.29 × 10−17 cm3 s−1) than that (2.87 × 10−17 cm3 s−1) in Y2O3, indicating that CaSc2O4 is an excellent host for achieving very intense UCL in Tm3+/Yb3+ codoped oxide upconverting materials.
No takes yet. Share an insight, caveat, or question.
Li et al. (2012) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: