This work is focussed at investigating the properties of additive manufactured Ti-6242S, a Ti alloy with excellent mechanical strength and stability up to 550 °C. Special attention is given to the effect of different heat treatment routes on microstructure and high-temperature mechanical behaviour of the Ti-6242S alloy produced by Laser Powder Bed Fusion. Annealing was performed in the α/β field (at 940 °C, 960 °C, 980 °C) or above the β transus (at 1050 °C). Annealing step was followed by Ar gas cooling and ageing at 595 °C. The as-built material exhibits high strength and anisotropic behaviour, showing lower fracture elongation in the direction parallel to the build platform. Heat treatments are responsible for a reduction of material strength but an increase in fracture elongation. Tensile tests at high temperature show that the best heat treatment for applications up to 300 °C is the annealing at 940 °C followed by Ar cooling and ageing. For applications at higher temperatures (namely 550 °C, 750 °C) the annealing step should be performed above the β transus temperature, at 1050 °C, to achieve the best tensile properties.
No takes yet. Share an insight, caveat, or question.
Casati et al. (2021) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: