Constructing a nanocomposite to introduce a coherent interface is an effective way to improve the property of thermoelectric material. Here, a series composites of Bi 0.48 Sb 1.52 Te 3 – x wt % Sb 2 Te 3 ( x = 0, 0.3, 0.5, 0.8, and 1.0) were synthesized, where the hydrothermally prepared Sb 2 Te 3 nanosheets were intimately wrapped in the solid-state-reacted Bi 0.48 Sb 1.52 Te 3 matrix. The formation of a coherent interface was observed and confirmed by the scanning electron microscopy characterization. As the Sb 2 Te 3 content was over 0.5 wt %, the carrier mobility could increase by 26%, while the carrier concentration decreased by 9% compared to those of the pure matrix at 300 K, enhancing the power factor to 40.1 μW/cm K 2 . Moreover, the Bi 0.48 Sb 1.52 Te 3 –0.5 wt % Sb 2 Te 3 sample exhibited a reduced lattice thermal conductivity of 0.83 W/m K at room temperature, resulting from the strengthened phonon scattering by interfaces. Combined with the manipulations of both the electronic and thermal transport by constructing a coherent interface, a maximum ZT of 1.05 was obtained in the x = 0.5 composite at 300 K, and it was improved by 20% compared with the result of the Bi 0.48 Sb 1.52 Te 3 matrix.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Shi et al. (2020) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: