Experimental evaluation demonstrates high fracture toughness in upscaled tungsten fibre-reinforced composites, suggesting their viability as resilient armour materials for fusion reactors.
Tungsten fibre-reinforced tungsten composites (Wf/W) have been in development to overcome the inherent brittleness of tungsten as one of the most promising candidate for the first wall and divertor armour material in a future fusion power plant. As the development of Wf/W continues, the fracture toughness of the composite is one of the main design drivers. In this contribution the efforts on size upscaling of Wf/W based on Chemical Vapour Deposition (CVD) is shown together with fracture mechanical tests of two different size samples of Wf/W produced by CVD. Three-point bending tests according to ASTM E399 for brittle materials were used to get a first estimation of the toughness. A provisional fracture toughness value of up to 346MPam1/2 was calculated for the as-fabricated material. As the material does not show a brittle fracture in the as-fabricated state, the J-Integral approach based on the ASTM E1820 was additionally applied for this state. A maximum value of the J-integral of 41kJ/m2 (134,8MPam1/2) was determined for the largest samples. Post mortem investigations were employed to detail the active mechanisms and crack propagation.
No takes yet. Share an insight, caveat, or question.
Schwalenberg et al. (2022) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: