Answers are grounded in this paper and cite their sources.
The room temperature tensile properties of nine high-strength aluminum-alloy sheet materials have been determined after elevated temperature exposures covering a range of times and temperatures suitable for elevated temperature forming. Times ranged from 5 to 20 min. at temperatures up to 500°F. I t is found tha t the naturally aged materials 24S-T, 24S-RT, and 61S-W may be exposed (without deformation) for 20 min. at temperatures up to a t least 500°F. with little or no loss in yield stress. Large increases may be expected at temperatures from 450° to 500°F. The artificially aged materials 24S-T81, 24ST84, 24S-T86, 61S-T, R301-T, and XB75S-T may be exposed as long as 20 min. (without deformation) at temperatures up to 400°F. with little or no loss in yield stress but above 450°F. the loss becomes great. Additional tests made on material taken from deep-drawn cups formed at 300° and 450°F. indicate that the deformations involved in hot forming may induce an acceleration of the elevated temperature aging process.
No takes yet. Share an insight, caveat, or question.
Lapsley et al. (1947) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: