This is the authors' abstract. We don't add key points for this paper.
The Na 5 Tm 1 − x (Y 1/3 Yb 2/3 ) x (MoO 4 ) 4 ceramics (x=0-0.18) were successfully synthesized via the solid-state reaction method. XRD analysis revealed that they possessed a single-phase tetragonal scheelite structure belonging to the space group I4₁/a(88). SEM analysis demonstrated that the samples sintered at 600 °C exhibited a dense microstructure, with a relative density as high as 94.9% and an average grain size ranging from 2.172 μm to 2.424 μm. The relative density serves as an external factor influencing ε r and Q×f, while τ f is related to bond valence. The ionicity of the Tm-O bond, and the lattice energy and bond energy of the Mo-O bond are the intrinsic factors determining ε r , Q×f, and τ f , respectively. Raman spectroscopy provided an intuitive characterization of the vibrational properties of the [MoO 4 ] 2− tetrahedra within the ceramics. Although the pure phase Na₅Tm(MoO 4 ) 4 ceramic exhibited optimal dielectric properties (ε r =8.025, Q×f=18,967 GHz, and τ f = -101 ppm/°C) at 625 °C, the Na 5 Tm 0.91 Y 0.03 Yb 0.06 (MoO 4 ) 4 ceramic sintered at 600 °C demonstrated superior dielectric properties (ε r =7.82, Q×f=34,752 GHz, and τ f = -71.9 ppm/°C).
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Chen et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: