We present a detailed investigation of sequential melting of the two components of isodimorphic poly[(butylene succinate)- ran -(butylene adipate)] (PBS- ran -PBA, or PBSA) having 40:60 and 50:50 compositions, located in the pseudoeutectic region, by using various NMR methods and in situ atomic force microscopy (AFM) after cooling from the melt at various cooling rates. In situ AFM measurements provide a direct evidence of the presence of two types of lamellar crystals (i.e., PBS-rich and PBA-rich crystal phases with different melting points) within the measured 40:60 PBSA copolymer, enabling us to directly observe the melting of the individual components. From analyses of 1 H low-resolution NMR free-induction decays, we quantify the composition of sample crystallinity and show that each component of PBSA contributes significantly differently to overall crystallinity, which is affected by the thermal history and composition. 13 C magic-angle spinning (MAS) NMR results indicate the inclusion of BS-units in the PBA-rich crystals for 40:60 PBSA, whereas only limited or no inclusion of BA-units in the PBS-rich phase is possible for both compositions under the given conditions. Our results once again showcase the use of combined low- and high-field MAS NMR techniques to quantify the comonomer inclusion in isodimorphic random copolymers under different crystallization conditions.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Tariq et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: