The new type of Gd-rich FeCrNiMo alloys with different Mo content was designed and fabricated. After cold rolling and solution treatment, the alloys contain austenite matrix and granular Ni 5 Gd phase. Ni 5 Gd phase has not undergone significant changes, while Sigma phase can gradually precipitate from the matrix during the long-term thermal aging at 600 °C. With increasing exposure time or Mo content, the number of Sigma phase and its size also gradually increases. The hardness and strength increased with the Mo addition, and the room-temperature fracture elongation of all alloys in the solid solution state is greater than 30 %. The ductile fracture type for all alloys before and after aging 5000 h have not changed. Increasing exposure time or Mo content enhanced the strength and hardness, while damaging the fracture elongation. When the Mo content is less than 1.5 wt%, the fracture elongation of alloy after aging 5000 h remains above 26 %. This study offers novel perspectives on function and structure integrated shielding alloy for long-term application in high-temperature environments.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Pan et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: