Martensite-austenite (M-A) constituent in the heat affected zone (HAZ) usually plays a detrimental role in toughness, especially in the intercritically reheated coarse-grained (ICCG) HAZ. However, its transformation mechanism has been rarely investigated. In the present study, transformation process of reverted austenite (γ r ) formed at different second pass peak temperatures ( T p2 ) was studied through interrupt quenching and multi-scale characterizations on decomposition products of γ r . And the correlation between transformation mechanism, final status (size, distribution and hardness) of M-A constituent and toughness deterioration was discussed. The results showed that distinct volume fraction and carbon enrichment of γ r formed at different T p2 determined subsequent phase transformation process. Lower T p2 induced small reverted fraction and higher carbon content of γ r , which continuously distributed along coarse grain boundaries, and the final M-A constituent inherited the continuous distribution and high carbon content of γ r , which yielded high M-A hardness and deteriorated the toughness. Higher T p2 triggered larger fraction of γ r with lower carbon content, and M-A constituent was subdivided or dispersed by decomposition product of γ r (ferrite, bainite and accicular ferrite). The size of M-A and decomposed products were also refined. Dispersed and refined M-A with lower hardness could notably mitigate the toughness deterioration of ICCGHAZ.
No takes yet. Share an insight, caveat, or question.
Li et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: