Processing of a CeO2 layer on an IBAD-Gd2Zr2O7 buffer tape was investigated as a cap layer. In the process of this study, we found that the CeO2 cap layer by the PLD method on the IBAD buffer tape brought about high in-plane grain alignment without Ar ion assistance such as the IBAD process. The Δφ value, degree of the in-plane grain alignment decreased from 25.4 degrees and 11.6 degrees for the IBAD-GZO to 4.9 degrees and 2.4 degrees for the PLD-CeO2, respectively. We call this phenomenon “self-epitaxial PLD-CeO2 cap layer”. Then, we suggested a new process which is a combination of a thin IBAD-GZO by short time deposition and a PLD-CeO2 with high rate deposition in order to enhance the fabrication rate for the buffer layer process. The new self-epitaxial process is very promising as a buffer layer process in terms of both high grain alignment and rapid fabrication.
No takes yet. Share an insight, caveat, or question.
Muroga et al. (2004) studied this question.
Synapse has enriched 5 related papers. Consider them for comparative context: