: The effect of different preheating treatments on the microstructure and corrosion properties of as-extruded Mg-9.5Gd-2.7Y-0.9Zn-0.8Cu-0.8Ni alloy applied as plugging tools are investigated in this work. The results show three alloys (named as ST1, ST2 and ST3 alloys) with different long-period stacking ordering (LPSO) phase contents which are 22.3%, 33.1% and 44.7%, respectively, are obtained by adjusting the preheat treatment before the hot extrusion. After undergoing hot extrusion, all ST-E alloys comprise both lamellar and block LPSO phases. The ST1-E alloy exhibits more lamellar LPSO phase and discontinuous block LPSO phase, along with the finest grain size among the three alloys. In terms of corrosion performance, the weight loss rates and electrochemistry analyses reveal that the ST1-E alloy displays the highest corrosion rate. It is primarily attributed to more favorable corrosion sites provided by the substantial multilayered structures (lamellar LPSO phase/Mg matrix/lamellar LPSO phase), effective galvanic corrosion effect induced by the discontinuous block LPSO phase and the Mg matrix, and smaller grain size. This work deepens the understanding of the effect preheat treatment process on the corrosion performance and provides a simple and available approach to regulate corrosion properties of the dissolvable Mg alloys containing the LPSO phase.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Liu et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: