In this study, the hydrogen embrittlement behavior of an ultrahigh strength mooring chain steel with a tensile strength of 1150 MPa was evaluated. The hydrogen was precharged into the notched specimen by electrochemical hydrogen charging. The fracture stress and hydrogen content were obtained by a slow strain rate test (SSRT) and thermal desorption analysis (TDA). The results show that the fracture stress decreased linearly with hydrogen content when the hydrogen content was less than 2.0 wppm. At this point, the intergranular fracture occurred, where the fracture stress as a function of hydrogen content changed from a linear to a power law relationship. The maximum hydrogen content from the corrosive environment was 1.4 wppm, which is lower than that of the onset of intergranular fracture at a diffusible hydrogen content of 2.0 wppm. The precharged hydrogen was possibly trapped by the grain boundaries.
No takes yet. Share an insight, caveat, or question.
Li et al. (2019) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: