This is the authors' abstract. We don't add key points for this paper.
In the present work, the fused deposition modeling (FDM) technique was used to produce PP/SEBS/SiO2 composite and optimize the melting temperature, yield strength, and impact strength of printed samples. The parameters of print speed, nozzle temperature, and SiO2 content were selected to study the thermal and mechanical behavior of the composite. Furthermore, the fracture surface of the printed parts was analyzed by SEM images. The results showed that the melting temperature of the composite was significantly enhanced (8.3%) by the addition of SiO2 nanoparticles, but with the increase of nozzle temperature and print speed, a slight change was observed in the melting temperature (1.8% and 1.2%). In addition, the improvement in the yield strength of the composite (33%) was obtained at SiO2 content of 2.5 wt%, because the particles were well distributed in the PP matrix. Also, the impact resistance of the composite was enhanced (30.2%) with the increase of print speed, while the increase of nozzle temperature and SiO2 content reduced the impact strength (15.3% and 23.3%). The concurrent enhancement of the melting temperature, yield strength, and impact resistance of the PP/SEBS/SiO2 composite was obtained by a print speed of 80 mm/s, a nozzle temperature of 240°C, and SiO2 content of 2.8 wt%.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Ghnim et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: