Answers are grounded in this paper and cite their sources.
A high density CaKFe 4 As 4 bulk sample was successfully synthesized using a spark plasma sintering (SPS) technique. The density of the synthesized sample was 5.02 g cm −3 , corresponding to 96.2% of the theoretical density of CaKFe 4 As 4 . Moreover, a reasonably high Vickers hardness of 1 GPa was measured. The electrical resistivity of the SPS bulk sample was as low as approximately 600 μ Ω cm at 300 K, which is smaller than that of the ordinary sintered polycrystalline sample by nearly one order of magnitude, and exhibited a sharp superconducting transition with the transition width (Δ T c ) less than 2 K, indicating an improved grain connectivity. The critical current density of the SPS bulk sample calculated from the magnetization hysteresis loops (magnetic J c ) reached 18 kA cm −2 at 4.2 K under 5 T, which is the highest among the iron-based superconductor polycrystalline samples reported thus far.
No takes yet. Share an insight, caveat, or question.
Ishida et al. (2020) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: