We fabricated CaKFe 4 As 4 round wires through a powder-in-tube method followed by hot isostatic pressing up to 175 MPa. The transport critical current density, J c , at 4.2 K almost reached the level for practical applications (100 kA cm −2 ) under self-field and reached 7.6 kA cm −2 at 100 kOe. Magneto-optical images confirmed that the grains were well-connected at low temperatures. Although high-pressure sintering at high temperatures enhanced the J c and density of the core of the wires, X-ray diffraction and scanning electron microscopy–energy-dispersive X-ray spectroscopy analyses indicated that impurity phases were present in both the polycrystalline powder and the core of the wire.