Answers are grounded in this paper and cite their sources.
A phosphor-in-glass film on sapphire (PiGoS) structure was fabricated by electrostatic spraying as a low-porosity, thickness-controllable color-conversion layer for LED fog-lamp applications. YAG:Ce 3+ phosphor and borosilicate glass powders were mixed at a weight ratio of 7:3, deposited onto 100-µm-thick sapphire substrates, sintered at 740 °C, and polished to thicknesses of 150–250 µm. Structural and optical analyses confirmed that the YAG:Ce 3+ crystalline phase and characteristic Ce 3+ emission were preserved after fabrication. Micro-CT results showed that the pore-volume fraction decreased from 8.7% in conventional PiG to 2.3% in PiGoS. The optimized 150 µm PiGoS achieved the highest luminous efficacy of 109.4 ± 3 lm/W, representing an approximately 8% improvement over the 150 µm PiG reference, with a 6.3% quantum-efficiency enhancement. As the PiGoS thickness increased from 150 to 250 µm, the calculated pore volume increased from 9.32 to 27.96 mm 3 , while the luminous efficacy decreased to 94.8 ± 3 lm/W. Wafer-level mapping further confirmed stable optical uniformity across diced PiGoS chips. These results demonstrate that electrostatically sprayed PiGoS is a promising wafer-scalable phosphor-conversion platform for high-efficiency LED fog lights.
No takes yet. Share an insight, caveat, or question.
Hsu et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: