Zinc oxide particles were prepared by heating zinc hydroxide precipitate in a mixed solution of H2O and ethanol at 348 K for 2 h. When the molar fraction of ethanol in the solution increased, the particle size of the obtained zinc oxide decreased. The band-gap absorption edge of the UV-VIS spectra of the obtained zinc oxide particles also shifted to the shorter wave length with an increase of ethanol molar fraction in the mixed solution. When zinc hydroxide was heated in pure ethanol, zinc oxide nanoparticles whose average diameter was 41 nm were obtained. The zinc oxide nanoparticles can be obtained by heat treatment of zinc hydroxide in the neutral solution at 348 K.