This is the authors' abstract. We don't add key points for this paper.
The continuous, random three-dimensional nanostructure of aerogels is the key determinant of their exceptional thermal insulating performance. However, at elevated temperatures, sintering can lead to disruption of this nanostructure. SiOC and SiZrOC aerogels were prepared by pyrolyzing organic–inorganic precursor aerogels at 1000 °C under an Ar atmosphere. The pyrolysis treatment resulted in the formation of a Si–O–C structure with excellent thermal stability. Following calcination at 1000 °C for 0.5 h, SiZrOC demonstrated a specific surface area retention rate of 76.8% and a pore volume retention rate of 75.8%, surpassing the most advanced ZrO 2 –SiO 2 aerogel. Additionally, SiZrOC consistently exhibited outstanding thermal insulation performance, with thermal conductivities of 0.0273 and 0.0332 W m –1 K –1 before and after calcination at 1000 °C, respectively. Notably, it was observed for the first time that the rearrangement of Si–C and Si–O bonds caused by pyrolysis induced a loosening effect on the SiO 4 structure within the aerogel. Consequently, during subsequent aerobic calcination, SiOC and SiZrOC underwent another phase separation stage, resulting in a further increase in the number of Si–O–C structures, which offers an approach to improve thermal insulation properties in extreme environments. The superior thermal stability and thermal insulation performance make SiZrOC a promising candidate for applications in high-temperature nanoscale thermal insulation materials.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Han et al. (2023) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: