Answers are grounded in this paper and cite their sources.
In this study, a high-Si ferritic/martensitic (F/M) steel thin-walled tube (T-Φ5) with an outer diameter of 5 mm and wall thickness of 0.5 mm were fabricated via Pilger cold rolling and intermediate annealing technology. The evolution of microstructure and texture during the process was characterized by various methods. Cold rolling induced the formation of typical α-fiber (<110>//AD) and γ-fiber (<111>//RD) textures in the tube. The subgrained microstructure formed after cold deformation underwent recrystallization during intermediate annealing at 800 ℃, resulting in reduced texture intensity in the recrystallized grains compared to the cold-rolled grains. The T-Φ5 tube subjected to final normalizing and tempering treatments exhibited low texture intensity and a fully martensitic lath microstructure. The average sizes of M 23 C 6 carbides and MX precipitates in the tube are 162.1 ± 59.7 nm and 42.8 ± 25.0 nm. The ultimate tensile strength and yield strength of T-Φ5 at room temperature are 815 MPa and 686 MPa, which decrease to 279 MPa and 247 MPa with increasing test temperature to 650 ℃. The total elongation shows a trend of “initial decrease followed by increase”, with a minimum value (17.5%) appearing at 400 ℃ dominated by dynamic strain aging (DSA) mechanism. The ln(dσ/dε) vs. lnσ curves obtained during tensile test reveal a significant temperature dependence in the strain hardening behavior of the tube, mainly due to the influence of DSA at medium temperatures and dislocation recovery/annihilation mechanisms at high temperatures. This work has a positive role for optimizing the processing and practical application of high-Si F/M steel cladding tubes.
No takes yet. Share an insight, caveat, or question.
Ren et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: