This study investigates C40 grade Low-Carbon Concretes (LCCs) and Alkali-Activated Low-Carbon Concretes (AALCCs) combining an 80% ternary blend of supplementary cementitious materials (SCMs) with 0-100% recycled coarse aggregate (RCA). The ternary blend of SCMs comprised of ground granulated blast furnace slag (GGBFS), fly ash (FA) and silica fume (SF), as an alternative to ordinary Portland cement (OPC). No activation was used for LCCs, while AALCCs were activated using a low dosage sodium metasilicate pentahydrate. Their fresh states, short to long-term mechanical properties (3-365 days), microstructural characteristics, embodied carbon emissions (ECE), and cost were investigated. Results demonstrated that though increasing RCA reduced fresh state and mechanical performances, declining rate was substantially lower for LCCs and AALCCs than conventional concretes. Both LCCs and AALCCs maintained required fresh state performance even at high RCA levels, while continuous hydration and pozzolanic reactions led gradual development of compressive strength and elastic modulus up to one year. At 100% RCA replacement, long-term reductions in compressive strength were limited to 5-7% and 8-12% for LCCs and AALCCs, respectively, compared with 32-43% for conventional concrete. Furthermore, LCCs incorporating 80-100% RCA and AALCCs containing 80% RCA achieved mechanical properties comparable to those of conventional C25-C32 concretes with natural aggregates. Microstructural observations were consistent with the RCA defects mitigation effects of GGBFS, FA, and SF which mitigated RCA defects through pore filling, matrix development, and micro-bridging without aggregate pre-treatment. Furthermore, the LCCs and AALCCs reduced ECE by 48-60% through combined substitution of SCMs and RCA.
No takes yet. Share an insight, caveat, or question.
Khan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: