Novel, volatile (fluoroalkylthiolato)tin(IV) precursors have been synthesised and (CF3CH2S)4Sn used to deposit tin sulfide films under APCVD (atmospheric pressure chemical vapour deposition) conditions. H2S is, however, required as co-reactant. Films deposited at 300–400 °C are composed of sulfur-deficient SnS2, films deposited at 450 and 500 °C comprise the sesquisulfide, Sn2S3, and the films deposited at 550 or 600 °C are sulfur-deficient SnS. The structure of [CF3(CF2)5CH2CH2S]4Sn is also reported.