To reduce the seed length while maintaining the advantages of the cuboid KDP-type crystal, a long-seed KDP crystal with size 471~mm× 480~mm× 400~mm is rapidly grown. With almost the same high cutting efficiency to obtain third harmonic generation oriented samples, this long-seed KDP-type crystal can be grown with a shorter seed than that of the cuboid KDP-type crystal. The full width at half maximum of the high-resolution X-ray diffraction of the (200) crystalline face is 28.8 arc seconds, indicating that the long-seed KDP crystal has good crystalline quality. In the wavelength range of 377–1022 nm, the transmittance of the long-seed KDP crystal is higher than 90%. The fluence for the 50% probability of laser-induced damage (LID) is 18.5~J/cm² (3 ns, 355 nm). Several test points survive when the laser fluence exceeds 30~J/cm² (3 ns, 355 nm), indicating the good LID performance of the long-seed KDP crystal. At present, the growth of a long-seed DKDP crystal is under way.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Chen et al. (2020) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: