Answers are grounded in this paper and cite their sources.
SiO/sub 2/ layers with thicknesses of 150 nm, 1 mu m, and 2.5 mu m were either thermally grown or made by chemical vapor deposition on silicon wafers. Negative and positive charging of the free SiO/sub 2/ surface was performed by means of liquid-contact, corona, and electron-beam methods. Partially penetrating electrons were used to charge the volume of 2.5- mu m-thick SiO/sub 2/ layers. The good charge stability of negatively charged SiO/sub 2/ is demonstrated in isothermal measurements at room temperature and at 350 degrees C as well as in TSD experiments. In the isothermal measurements, positively charged samples showed a somewhat faster decay than negatively charged ones. The decay curves of negatively charged samples at elevated temperature can be interpreted with a simple theory based on carrier drift and compensation by conductivity. In the measured TSD spectra, the difference between differently charged samples is that the main peak of a positively charged sample appears at a much lower temperature than the peak of a negatively charged one. Samples positively charged with the corona or liquid contact method also show lower peak performance temperatures than samples positively charged with the electron-beam method.>
No takes yet. Share an insight, caveat, or question.
P. Günther (1989) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: