This is the authors' abstract. We don't add key points for this paper.
Crystallization behavior and morphology of PLA blended with 0.05–1.00 wt % loadings of poly( D -lactic acid) (PDLA) forming stereocomplex crystallites as in-situ nucleating agents, were studied using wideangle X-ray diffraction (WAXD), differential scanning calorimetry (DSC), and polarizing-light optical microscopy (POM). Blending PLA with small amount of PDLA does lead to formation of PLA stereocomplex (SC), although the PLA is a random copolymer. The in-situ formed SC crystal acted as nucleation sites in blends and accelerated the crystallization of PLA by decreasing the half-time ( t 1/2 ). The nucleation efficiency of PDLA obviously increased and the crystallization induction time decreased while the content of PDLA reached up to 0.20 wt %. While the content of PDLA is 0.2 wt %, the nucleation efficiency of PDLA is up to 43.8%, and the induction time decreased from 430 to 88 s. In addition, compared with pure PLA, t 1/2 decreases from 15.1 to 3.5 min at T c = 127.5°C while the amount PDLA is 1.0 wt %. The equilibrium melting temperature of PLA decreased from 187.2 to 181.2°C with the increase of PDLA content.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Zou et al. (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: