Answers are grounded in this paper and cite their sources.
Low friction mechanism of hydrogenated Diamond-Like Carbon (a-C:H) was assumed that sp^3 structures were destructed to graphite-like having low shearing strength. However, these structural changes generally occur when a-C:H coating was rubbed during several thousand cycles so-called running-in process. However, long running-in process is not necessaly. So it is required to obtain low friction surface by a substitute process. From the view point of reformation of structure, we focused on ultraviolet ray (UV) irradiation. It was assumed that UV was able to destruct the a-C:H topmost surface to graphite-like when the ray intensity exceeded C-C single bond energy, and generated dangling bonds were assumed to combine. We prepared PECVD a-C:H coatings which were irradiated with UV of 254, 312, and 365nm wavelengths for 60min. These specimens and asdeposited a-C:H were tested with a ball-on-disk type friction tester, operating at 0.084m/s and 0.1N, and counter material was Si_3N_4 balls with 8mm diameter. During 250 to 4500 cycles, friction coefficient of 254 and 312nm UV irradiated a-C:H exhibited 0.02 to 0.05, which value was less than that of un-irradiated a-C:H. 254 and 312nm UV irradiated a-C:H exhibited similar C KLL peak to HOPG (Highly Oriented Pyrolytic Graphite). The hardness of UV irradiated a-C:H changed from 11.5 to 13.1GPa. Moreover, the surface roughness of each a-C:H did not change by UV irradiation. These results indicated that a structural change in the topmost surface to graphite-like structure was an important roll to obtain low friction coefficient.
No takes yet. Share an insight, caveat, or question.
TOKOROYAMA et al. (2010) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: