Shear stress vs. shear strain curves have been obtained from magnesium single crystals orientated for basal glide and tested in tension over the temperature range 77 to 413 °K. Incremental changes of strain rate and temperature were also made and the results used to deduce the usual parameters of thermally activated flow. A two‐stage hardening curve was found, the work‐hardening rate being 150 to 400 g/mm2 in stage I at room temperature, and 3 to 5 kg/mm2 in stage II. The Cottrell‐Stokes law was found to be obeyed for strain rate changes at low temperatures, but at higher temperatures the behaviour was more complex. The activation energy for stage I deformation increased to a roughly constant value of 0.3 to 0.4 eV at high temperatures.