This is the authors' abstract. We don't add key points for this paper.
In this paper, we aimed to improve the oxidation and ablation resistance of carbon fiber-reinforced carbon (CFC) composites at temperatures above 2000 °C. C/C–SiC–ZrB2 ultra-high temperature ceramic composites were fabricated through a complicated liquid–solid reactive process combining slurry infiltration (SI) and reactive melt infiltration (RMI). A liquid Si–Zr10 eutectic alloy was introduced, at 1600 °C, into porous CFC composites containing two kinds of boride particles (B4C and ZrB2, respectively) to form a SiC–ZrB2 matrix. The effects and mechanism of the introduced B4C and ZrB2 particles on the formation reaction and microstructure of the final C/C–SiC–ZrB2 composites were investigated in detail. It was found that the composite obtained from a C/C–B4C preform displayed a porous and loose structure, and the formed SiC–ZrB2 matrix distributed heterogeneously in the composite due to the asynchronous generation of the SiC and ZrB2 ceramics. However, the C/C–SiC–ZrB2 composite, prepared from a C/C–ZrB2 preform, showed a very dense matrix between the fiber bundles, and elongated plate-like ZrB2 ceramics appeared in the matrix, which were derived from the dissolution–diffusion–precipitation mechanism of the ZrB2 clusters. The latter composite exhibited a relatively higher ZrB2 content (9.51%) and bulk density (2.82 g/cm3), along with lower open porosity (3.43%), which endowed this novel composite with good mechanical properties, including pseudo-plastic fracture behavior.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Sun et al. (2021) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: