采用水热法制备了Gd2O3:Er/Yb纳米线,使用980 nm和488 nm激光作为激发光源,研究了Gd2O3:Er/Yb纳米线的上转换和下转换发光特性。研究发现,随着激发功率密度的增大和温度的升高,2H11/2-4I15/2和4S3/2-4I15/2的发射强度之比明显增大,这种现象被归因于电子的热激活速率增大,2H11/2和4S3/2能级上的电子布居数的改变。 The Gd2O3: Er/Yb nanowires were prepared by the hydrothermal method. Luminescence properties, mechanism and dependence of luminescence intensity on pump power density were researched. In Gd2O3:Er/Yb nanowires, the intensity ratio of 2H11/2-4I15/2 to 4S3/2-4I15/2 increased dramatically with the pump power increasing, which was attributed to the increase of thermal populations in 2H11/2 energy level caused by irradiation induced temperature increase.