When grown in a nonanoic acid-limited chemostat at a dilution rate of 0.25 h(-1), Pseudomonas putida KT2440 produced poly(3-hydroxynonanoate-co-3-hydroxyheptanoate) containing 68 mol % 3-hydroxynonanoate (C9) and 32 mol % 3-hydroxyheptanoate (C7). Under the same conditions, but in the presence of acrylic acid, a fatty acid β-oxidation inhibitor, the C9 monomer content increased to 88 mol %. Cofeeding glucose (3.9 g L(-1)) and nonanoic acid (2.9 ± 0.1 g L(-1)) in continuous culture with 0.2 g L(-1) of acrylic acid in the feed, further increased the C9 content to 95 mol %. A yield of PHA from nonanoic acid of 0.93 mol mol(-1) was attained. PHA with a 3-hydroxyoctanoate (C8) content of 98 mol % was produced with the same cofeeding methodology from octanoic acid. As the dominant monomer content increased, the melting point of the poly(3-hydroxynonanoate) copolymers increased from 46 to 63 °C and that of the poly(3-hydroxyoctanoate) copolymers from 54 to 62 °C. All copolymer compositions resulted in elongation to break values of about 1300%, but tensile strength at break and Young's modulus both increased with increasing amounts of the dominant monomer.
No takes yet. Share an insight, caveat, or question.
Jiang et al. (2012) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: