This is the authors' abstract. We don't add key points for this paper.
In powder-in-tube processed MgB 2 wires, the choice of boron powder as a starting material crucially affects their performance. In this paper, we prepared in situ MgB 2 wires from three types of boron powders in various heat-treatment conditions and investigated their electromagnetic properties and microstructures. Their critical current density, J c , varied over a wide range from sample to sample. The difference in J c is understood to be caused by the effect of changes in the electrical connectivity, K , and intrinsic residual resistivity, ρ 0 . Here, K represents the effective cross-sectional area for current, and ρ 0 reflects the degree of the charge carrier scattering caused by lattice defects. It was found that the use of boron powder with a large specific surface area leads to a large degree of lattice defects in MgB 2 grains and enhances ρ 0 , resulting in improving J c . The boron powder produced by thermal decomposition of B 2 H 6 has a large specific surface area. Hence, this boron powder is the most suitable as a starting material for MgB 2 . Meanwhile, dry pulverization of low-cost boron powder, which is largely produced by active-metal reduction of B 2 O 3 , is also effective to increase its specific surface area without introducing impurities, resulting in the enhancement of J c in the entire magnetic field region. This finding broadens the choice of boron powder and contributes to realizing superconducting applications with excellent balance between performance and cost.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Kodama et al. (2016) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: