Answers are grounded in this paper and cite their sources.
CuO added Pb 0.92 Sr 0.06 Ba 0.02 (Mg 1/3 Nb 2/3 ) 0.25 (Ti 0.53 Zr 0.47 ) 0.75 O 3 ceramics were studied to prepare high-quality multilayer piezoelectric actuators with pure Ag electrodes at 900°C. CuO addition not only reduced the sintering temperature significantly from 1260°C to 900 °C but also improved the ceramic density to 7.742 g/cm 3 . The 0.7 wt.% CuO added ceramic sintered at 900 °C shows the remnant polarization ( P r ) of 40 µC/cm 2 , 0.28% strain at 40 kV/cm, and the piezoelectric coefficient ( d 33 ) of 630 pC/N. This ceramic shows a strong relaxor characteristic with a Curie temperature of 200 °C. Furthermore, the 0.7 wt.% CuO added ceramic and pure Ag electrodes were co-fired at 900 °C to prepare a high-quality multilayer piezoelectric actuator with a d 33 of over 450 pC/N per ceramic layer.
No takes yet. Share an insight, caveat, or question.
Qaiser et al. (2017) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: