Answers are grounded in this paper and cite their sources.
Semi‐crystalline potassium titanates, useful as precursors to produce composite materials and coatings, were synthesized by thermal treatment of powdered TiO 2 in molten mixtures of KNO 3 and KOH at 450°–550°C. The products obtained had similar structures of laminar crystals, aggregated in particles of about 3 μm of n =TiO 2 /K 2 O molar ratio in the range 2.8–6.0. The value of n could be regulated by the temperature of synthesis, the weight ratio of [KOH]/[KNO 3 ] in the molten salt mixture, and the number of water washing operations. The reduction of the TiO 2 /K 2 O molar ratio increased the contents of H 2 O in the composition of potassium polytitanate, from 5.3 to 11.4 and from 0.2 to 8.6 (wt%) in the adsorbed and structural forms. The thermal treatment of the potassium polytitanate precursors obtained resulted in dehydration and chemical interaction with unreacted TiO 2 at 500°–750°C, amorphization at 750°–850°C, crystallization of K 2 Ti 4 O 9 (in some cases K 3 Ti 8 O 17 ) at 850°–1090°C, and crystallization of K 2 Ti 6 O 13 at temperatures >1090°C. The mechanisms of the structural transformation and phase evolution were considered as a function of the TiO 2 /K 2 O molar ratio in the potassium polytitanate.
No takes yet. Share an insight, caveat, or question.
Sanchez‐Monjaras et al. (2008) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: