Zinc oxide nanostructures have been successfully prepared through dissolving of microsized zinc xide powder in ammonium hydrogencarbonate solution at 25°C, followed by calcination of the resultant precipitates at 350°C for 1 h. The influence of urea presence on morphology and particle size of the as-prepared zinc oxide was also investigated. The obtained products were characterized by XRD, SEM, FT-IR, UV-Vis, and Brunauer–Emmett–Teller (BET) N2 adsorption method. The results revealed that the morphology of the as-prepared ZnO samples is susceptible to the reactant conditions. It was found that the crystallite size of the prepared samples decreases by increasing of ammonium hydrogencarbonate, urea, and ZnO amount.