To improve the performance of elastic current-carrying friction pairs, this study employs a wire–plate friction pair and investigates the effect of surface texture orientation on current-carrying friction performance using a self-made micro-sliding current-carrying friction wear tester. The following conclusions were drawn: The angle between texture orientation and friction direction primarily influences the friction pair’s lifespan. At 0°, the lifespan is the longest, exceeding 500 cycles, followed by 90° with a lifespan of 394 cycles, and the shortest lifespan is observed with multi-directional textures. The primary wear mechanisms during the lifespan are furrowing, adhesive tearing, arc erosion, oxidation, and material transfer. At 0°, the width of mechanical damage is confined to the furrows, and the arc erosion is minimal. At 90°, the mechanical damage width and arc erosion are moderate, while at 45°, 135°, and multi-directional orientations, the mechanical wear width and arc erosion are more severe, with the multi-directional texture having the widest mechanical wear. The texture orientation has a significant impact on the performance and running process of current-carrying friction pairs. An appropriate texture orientation can suppress wear, thereby enhance performance and extending service life.
No takes yet. Share an insight, caveat, or question.
Yang et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: