A study is conducted on the flow stress behavior of the spray-deposition processed 17 vol% SiC p /7055Al composite through hot compression tests at the temperatures ranging from 250 °C to 450 °C and the strain rates of 0.001–1 s −1 , including microstructure evolution . As indicated by the calculation results, the deformation activation energy for the SiC p /7055Al composite is 145.28 kJ/mol. All of the obtained flow curves are characterized by dynamic recovery and/or dynamic recrystallization . The hot deformation of the composites in the temperature range of 250–350 °C and strain rate region of 1–0.001 s −1 exhibited the typical characteristics of dynamic recovery. As the deformation temperature increases, the deformation mechanism of the composites shifted to dynamic recrystallization over time. The flow stress showed a decreasing trend with the increase of deformation temperature and the decrease of strain rate, as reflected by a Zener–Hollomon parameter in hyperbolic sine equation. According to the processing map, the optimum hot workability domain is the peak region located around 430–450 °C and 0.001–0.03 s −1 . In addition, the orientation distribution function ODFs were calculated according to the pole figures, which revealed that the textures of the composites are significantly different at the varied hot deformation parameters.
No takes yet. Share an insight, caveat, or question.
Tang et al. (2020) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: