This study investigates the factors limiting the fracture strength of ultrafine-grained WC-Co cemented carbides, focusing on the roles of grain size, carbon content, and grain growth inhibitors (VC and Cr 3 C 2 ). WC-Co alloys with varying grain sizes (0.6, 0.4, and 0.3 μm) and inhibitor compositions were prepared. The relationship between transverse rupture strength ( TRS ) and defect size was analyzed using Suzuki-type and Almond-type plots. While the essential strength ( σ 0 ) increased with grain refinement obeying the Hall-Petch relationship, the limiting strength ( σ L ) exhibited a peak at 0.4 μm (WC04) and decreased for the finest 0.3 μm alloy (WC03). Detailed analysis revealed that the limiting strength is influenced by the carbon balance; specifically, lower carbon contents within the two-phase region improved the strength. However, the primary factor for the strength degradation in the finest grade was identified as the excessive addition of inhibitors. High dosages of VC and Cr 3 C 2 , required for extreme refinement, led to the formation of (V,W)C precipitates at WC/Co interfaces, which reduced the interfacial bonding strength. It is concluded that simply increasing the inhibitor amount does not guarantee high strength; instead, achieving grain refinement without forming strength-degrading precipitates is essential for realizing the potential of ultrafine-grained cemented carbides.
No takes yet. Share an insight, caveat, or question.
Kawakami et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: