Binary AlSn (1, 2, 4, 6, 8 at.%Sn) synthetic alloys were prepared under vacuum-atmosphere controlled furnace.The AlSn alloys were coated by plasma electrolytic oxidation technique for 120 min in aqueous electrolyte containing sodium silicate and potassium hydroxide using the same electrical parameters.The microstructure, surface roughness, phase content and chemical composition of the coatings were characterized by scanning electron microscopy, prolometry and X-ray diractometry.The coating became porous while coating thickness and surface roughness decreased, with increasing amount of Sn content in AlSn alloys.The coating was not formed on the AlSn alloy with 8 at.%Sn.Plasma electrolytic oxidation coatings were composed of mainly mullite (3Al2O3•2SiO2), γ-Al2O3 and α-Al2O3 up to 4 at.%Sn.The α-Al2O3 phase formed as precipitate in the inner region of the coating and its amount decreased with Sn amount in the AlSn alloys.The SnO2 phase was only detected in the coating of Al6Sn alloy.Scanning electron microscopy energy dispersive X-ray spectroscopy results showed that the traces of Sn were evident in the oxide coating along with Al, O, Si, Na, and K.The increasing addition of Sn in the alloys resulted in reduction of the overall microhardness of the coating with decreasing manner from dense inner region to the surface of the coatings.
No takes yet. Share an insight, caveat, or question.
Gençer et al. (2014) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: