Jatropha seed meal was extracted with n-hexane and the oil obtained was found to have iodine val ue 157.37, acid value 5,61 and free fatty acid 2.70. The fatty acid profile of the oil showed that oleic acid (3 1.35 %), palmitic acid (20.9 %) stearic acid (15.68 %) and caprylic acid (10.45 %) were the major fatty acid components. The seed oil was epoxidised at 29°C using peracetic acid produced in situ by reacting hydrogen peroxide (30 % vlv ) wi th various amounts of glacial acetic acid. Barium, cadmium, lead and zinc soaps of the oils were prepared by metathesis in alcohol solution. Thermal degradation studies on poly (vinyl chloride) in the presence of Jati'Opha seed oil, the epoxidised oil and the metal soaps of the oil s were carried out at various temperatures (170, 180 and 190°C) under ox idati ve and non-oxidative conditions. Changes in intrinsic viscosity and levels of unsaturation in the degraded polymer samples together with kinetic data (rate measurements at 1% conversion) were used to evaluate the relative stabili sing effect of the additives on the thermal degradation of poly (vinyl chloride). It was found that although the values of the rate of dehydrochlorination were of about the same order of magnitude (10- 2 % min· the rates were relatively lower, and the time at which degradation reached 1 % conversion considerably higher than the corresponding values obtained in the ·absence of the additives. The data from solution viscosity measurements and from estimates of the level of unsaturation in the degraded polymer samples indicate that metal soaps of the oil exert stabilising effect on the oxidative and monoxidative thermal degradation of poly (v inyl chloride). Th e low th ermal stabil it y of poly (v in yl chl oride), PVC is one of th e inherent problems associated with the manufacture and use of th e polymer. At elevated temperat ures , well below its decomposition temperature, PVC loses HCI , and becomes colourl ess , lea din g to changes 111 chemical and physical properties of th e polymer. Thermal degradation of PVC is genera ll y considered to be initiated at un stab le st ructural irregular sites (particu larly tertiary and allylic ch lori des) within PVC; and so me auth ors 1 5
No takes yet. Share an insight, caveat, or question.
FE Okieimen (2006) studied this question.
Synapse has enriched 9 related papers. Consider them for comparative context: