The thermoelectric properties of Y-doped polycrystalline SrTiO3 (Sr1-x Y x TiO3) are measured from 10 K to 900 K. The Y component is doped up to the solubility limit of Sr1-x Y x TiO3, x=0.1. The Y-doped polycrystalline samples show a low resistivity, ∼1 ×10-5 Ω·m and a large absolute value of the Seebeck coefficient, ∼150 µV/K, at room temperature. Consequently, they have a high power factor, 1.2 ×10-3 W/mK2, defined as PF=S 2/ρ, where S is the Seebeck coefficient and ρ is the resistivity. Furthermore, we observe a decrease in the thermal conductivity of SrTiO3 due to phonon scattering by the Y dopant.