The atomic structure of amorphous sulfate hardwood pulp obtained via regeneration in a dimethyl acetamide–LiCl solution is studied with the use of X-ray diffraction and computer simulation. When dimethyl acetamide appears within a cellulose chain, it becomes swollen. A chosen cluster has a complex structure and contains two cellulose chains II distorted by twisting and bending and two chains deformed by dimethyl acetamide molecules. A cluster with the formula unit (C 6 O 5 H 8.5 Li 1.5 ) • (H 2 O) 2.8 is obtained after relaxation with the addition of water. The uncertainty-profile factor for the model and experimental curves of X-ray scattering intensity distribution I ( s ) is 8%, and the distribution curve of s -weighted interference function H ( s ) calculated for the model best fits the experimental curve.