Answers are grounded in this paper and cite their sources.
The hot deformation behavior of TA32 titanium alloy in the temperature range of 650–850 °C and strain rate range of 0.0001–0.1 s−1 was studied by isothermal hot tensile tests conducted on an electronic universal testing machine equipped with an environmental chamber. The effects of temperature and strain rate on the flow stress of TA32 were investigated. Moreover, a back-propagation artificial neural network (BP-ANN) model was developed to predict the flow stress at elevated temperatures and three-dimensional (3-d) thermal processing maps. The results show that the three-layer BP-ANN model can precisely predict the flow stress as the correlation coefficient reaches 0.99365 and the mean relative error is 1.15621%. The 3-d thermal processing maps demonstrate that the lower strain rate, higher temperature, and larger strain lead to higher power dissipation efficiency and better formability. And it shows a flow instability tendency at lower temperatures and higher strain rates. Based on the 3-d thermal processing maps and microstructure analysis, the optimized temperature range and strain rate range for TA32 hot forming were 770–830 °C and 0.0001–0.00015 s−1.
No takes yet. Share an insight, caveat, or question.
Hu et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: