Answers are grounded in this paper and cite their sources.
The tempering characteristics of 8 cold work die steels containing 0.6 to 1.5% C, 5 to 12% Cr, 1Mo, and 0.3V were investigated by measurements of tempered hardness after quenching or subzero treating, volume fraction of retained austenite, and by identification of precipitated carbides. The effect of C and Cr on the hardness of the steel tempered at higher temperature is summarized below, (1) The effect of vol.% of retained austenite on the amount of secondary hardening of the steels is expressed by the following equations through the parameter, K=[%Cr]-6.8×[%C]H=0.25Vγ+C, Vγ=15.2-1.05K±1.5Where H (HRC) is the amount of secordary hardening for each alloy quenched from various austenitizing temperatures, Vγ (%) is the vol.% of retained austenite in the sample, and C is a constant.(2) With increasing parameter K, the amount of secondary hardening is increased by the precipitation of M7C3 carbides.(3) With increasing parameter, L=[%Cr]+15.5×[%C], the maximum tempered hardness increases.
No takes yet. Share an insight, caveat, or question.
Itoh et al. (1984) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: