This work investigates PLA-based biocomposites plasticized with 10 wt% maleinized corn oil (MCO) and reinforced with silk fibroin microparticles (SFM, 0.25–3 phr). Mechanical, thermal, and disintegration behavior were evaluated using standardized testing, FE-SEM, DSC/TGA, and Raman spectroscopy. MCO increased PLA ductility, raising elongation at break from 2.1% (PLA) to 6.3% (PLA-MCO), while decreasing tensile strength from 62.2 to 54.5 MPa. SFM provided a marked toughening effect at intermediate loading, reaching 37.0% elongation at break and 50.8 kJ·m⁻² impact energy for PLA-MCO-1SFM. However, higher SFM content (3 phr) reduced elongation to 28.8% and tensile strength to 44.9 MPa, suggesting limited compatibility. Thermal stability improved with MCO and SFM, with T5% increasing from 305.0 °C (PLA) to 326–333 °C. Disintegration tests showed that SFM delayed the disintegration rate under simulated composting conditions. Overall, combining MCO and controlled SFM loading enables tuning the mechanical and thermal performance of PLA-based materials.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Ferri et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: