Simultaneously improving the fire safety and mechanical performance of epoxy resin (EP) remains challenging because conventional additive flame retardants often require high loadings and impair network integrity. Herein, a phosphorus/nitrogen/silicon‐containing Schiff‐base‐derived flame retardant (DPSD) was synthesized and incorporated into an E‐51/DDM epoxy system. At 4 wt% DPSD, EP/DPSD‐4 achieved a UL‐94 V‐0 rating and an LOI of 30.7%, while impact strength increased by 59.5%. At 6 wt% DPSD, corresponding to only 0.33 wt% phosphorus, the LOI increased to 32.7%; PHRR and THR decreased by 37.2% and 32.3%, respectively, and PSPR and TSP decreased by 32.3% and 35.6%. Meanwhile, tensile strength increased by 40.3%. Char‐residue analyses revealed a compact, continuous, and more ordered phosphorus/silicon‐enriched protective layer, while TG‐FTIR showed suppressed evolution of combustible hydrocarbon and aromatic volatiles. These results indicate that DPSD promotes condensed‐phase charring and barrier effects, with a possible additional contribution from gas‐phase inhibition. The combined rigid aromatic units, polar groups, and flexible SiO linkages enable a favorable balance between network reinforcement and energy dissipation, providing a low‐phosphorus strategy for fire‐safe, strong, and tough epoxy thermosets.
No takes yet. Share an insight, caveat, or question.
Xinlei et al. (2026) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: