Answers are grounded in this paper and cite their sources.
This study evaluates pack boriding as an alternative to induction surface hardening in the manufacture of highly stressed tubular components exposed to combined mechanical, thermal and tribological loading, using the low-alloy Cr–V steel STN 15 230 as a model material. Test specimens were treated by induction surface hardening and by four pack-boriding regimes (800 °C/4 h, 900 °C/4 h, 900 °C/6 h and 1000 °C/4 h), each subset optionally followed by quenching and tempering. Boriding produced layers of 22–74 μm at 800–900 °C and 71 μm at 1000 °C; after subsequent quenching and tempering, the layer thickness shifted to 20–51 μm at lower temperatures but grew to 87 μm for the 1000 °C regime, indicating that stability during Q&T depends critically on the boriding conditions. The measured surface hardness of 1380–1720 HV 0.04 exceeded induction hardening (approximately 600 HV) by 2.3–2.9 times. A semi-empirical design methodology is proposed that couples steel chemistry, boriding parameters, and heat-treatment conditions through a boriding response index (BRI), a layer-thickness prediction, a thermal reserve factor (TR), and a stability index (SI). Applied to the four regimes tested, the SI ≥ 1.5 criterion correctly identified the stable (B2, B4) and unstable (B1, B3) processing routes and provides a basis for preliminary assessment of a proposed processing route prior to experimental verification.
No takes yet. Share an insight, caveat, or question.
Pastirčák et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: