To mitigate interconnect corrosion in seawater-fed solid oxide electrolysis cells (SOECs), Mn 1.5 Co 1.5 O 4 spinel coatings were deposited on Fe-22Cr stainless steel. At 750 °C, the coated interconnects exhibited an area-specific resistance (ASR) of 31.8 mΩ cm 2 after 4835 h of oxidation in air, with a parabolic rate constant of 3.0 × 10 −5 mg 2 cm −4 h −1 . Following exposure to seawater vapor for 500 h, the ASR reached 3.36 mΩ cm 2 , with a predicted value of 9.80 mΩ cm 2 at 5000 h. These findings underscore the coating’s improved oxidation resistance under dual-atmosphere conditions. Furthermore, a three-cells stack demonstrated high stability with a low degradation rate of 1.04 × 10 −5 h −1 at 100 mA cm −2 for 100 h. Post-test analysis confirmed a crack-free structure with negligible additional resistance, indicating that the spinel coating satisfies the engineering requirements for durable, direct seawater electrolysis and provides a scalable pathway for green hydrogen production.
No takes yet. Share an insight, caveat, or question.
Xie et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: