Answers are grounded in this paper and cite their sources.
The dry sliding wear behavior of martensitic stainless steel subjected to four heat-treatment processes (H950, H990, H1030, and H1070) was systematically investigated at loads of 50, 75, and 100 N. Results showed that the H990 specimen exhibited the highest hardness and impact toughness (IT). While the other three specimens possessed comparable hardness, their IT decreased with increasing heat-treatment temperature. At 50 N, H950 exhibited significantly higher wear volume than the others, due to coarse M23C6 carbides at grain boundaries, with the mechanism dominated by abrasive wear accompanied by plastic deformation and carbide spalling. As the load increased to 100 N, the wear volumes of H1030 and H1070 surpassed that of H950 due to their limited IT, as the mechanism transitioned to delamination wear driven by subsurface fatigue crack propagation. In contrast, H990 maintained the lowest wear volume throughout, attributed to its superior strength-toughness synergy. Specifically, high hardness effectively resisted abrasive cutting, while high toughness mitigated delamination wear by blunting crack tips and hindering crack propagation. These findings demonstrate that with increasing load, the dominant factor governing wear shifts from carbide characteristics to IT.
No takes yet. Share an insight, caveat, or question.
Jia et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: